Link Search Menu Expand Document
Converted document
 Subsubsection 4.2.2.2: Fiber with Neo-Hookean Law Uncoupled Up Subsection 4.2.2: Uncoupled Fiber Models Section 4.3: Continuous Fiber Distribution 

4.2.2.3 Fiber with Toe-Linear Response, Uncoupled Formulation

This material type is “fiber-pow-linear-uncoupled”. The following material parameters need to be defined:
<E> the fiber modulus in the linear range ( [P]
<beta> the power-law exponent in the toe region ( [ ]
<lam0> the stretch ratio when the toe region transitions to the linear region ( [ ]
The fiber strain energy density is given by where , Example:
Fiber model as specified in a solid mixture (Section 4.1.2.14↑)
<solid type="fiber-pow-linear-uncoupled">
  <fiber type="angles">
    <theta>20</center>
    <phi>90</phi>
  </fiber>
  <E>1</E>
  <beta>2.5</beta>
  <lam0>1.06</lam0>
</solid>